PRODUCTS

High permeability cathodic electrophoretic paint

High permeability cathodic electrophoretic paint

KD-312A phosphating solution, electrophoresis pretreatment solution

KD-312A phosphating solution, electrophoresis pretreatment solution

KD-331 surface conditioning agent, electrophoresis pretreatment agent

KD-331 surface conditioning agent, electrophoresis pretreatment agent

Matte Black Interior Solutions

Matte Black Interior Solutions

Particles generated during electrophoresis process

2025-05-15
1 Phenomenon
On the surface of the electrophoretic coating after drying, there are rough and hard particles or visible small blisters, which are often more severe in the horizontal plane than in the vertical plane of the coated material. These paint film defects are called particles.
2 Causes
1) The pH value of the tank solution is too high, and alkaline substances are mixed in, causing instability of the tank solution and resin precipitation or coagulation.
2) There are sedimentation "dead corners" and exposed metal areas in the groove.
3) The cleaning solution after electrophoresis is dirty and has a high paint content, resulting in poor filtration.
4) The surface of the object being coated and the lifting equipment entering are not clean, and the water washing after phosphating is poor.
5) During the drying process, granular dirt falls on the surface.
6) The coating environment is dirty.
7) Poor dissolution of paint or resin supply, with particles
CONTACT US
CONTACT US

IF YOU REQUIRE THE MOST SUITABLE PRODUCTS, FEEL FREE TO CONTACT US.

If you have any questions about our products or services, feel free to reach out to customer service team.
Code

INQUIRY

Code
Choose a different language
Current language: